Change search
Link to record
Permanent link

Direct link
Publications (10 of 12) Show all publications
Gustafsson, M., Junling, M., Eriksson, O. & Gudmundsson, A. (2023). Indikativ metod för bedömning av partikelemission från dubbdäcksslitage av vägbeläggning: modifiering och utvärdering av Tröger-metoden. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Indikativ metod för bedömning av partikelemission från dubbdäcksslitage av vägbeläggning: modifiering och utvärdering av Tröger-metoden
2023 (Swedish)Report (Other academic)
Alternative title[en]
Indicative test method for estimation of particle emission from studded tyre wear of road pavement : modification and assessment of the Tröger method
Abstract [sv]

Att testa partikelemissionen från dubbdäcksslitage av vägbeläggningar på ett kontrollerat sätt är oftast förknippat med verklighetsnära, men storskaliga tester med storskalig och avancerad laboratorie[1]utrustning och därmed förhållandevis höga kostnader. Det finns därför ett angeläget behov av en enklare metod som kan användas för att ge en rimlig och god skattning av hur skillnader i beläggningsrecept påverkar partikelbildningen, som kan användas till val av beläggningsrecept som ska användas i senare storskaliga tester. En möjlighet är att använda en befintlig slitagetestmetod för provkroppar av slitlager. Tröger är en sådan metod där ett knippe stålnålar hamrar mot en roterande provkropp i ett klimatskåp som bedömds lämplig för att mäta och studera partikelemissioner till luft. VTI:s Tröger-utrustning modifierades för partikelemissionsmätningar genom att installera partikelinsugsmunstycke i kylluftflödet som passerar över provkroppen. Initiala tester tydde på acceptabel/tillräcklig god repeterbarhet och ett antal provkroppar från några befintliga material med olika slitstyrka valdes ut för vidare tester. En statistiskt optimerad försökplan och provhantering togs fram. En testomgång var planerad initialt men senare utökades det till två omgångar. En andra omgång krävdes dels på grund av att ett material i första omgången misstagits för enhetligt, men bestod av tre olika material, dels då försöksuppställningen kunnat förbättras något. De bildade partiklarna (PM10) har en bimodal fördelning med en primär topp vid 2–3 µm och en sekundär vid ca 8–10 µm. Den statistiska analysen visade på signifikanta skillnader mellan de tre ingående materialen i provkropparna i den andra testomgången och att metoden i sin nuvarande form kan användas för att skilja partikelemissionen från olika vägbeläggningar. Förslag för att utveckla metoden är bland annat att förhindra uppbyggnad av damm i kylsystemet och säkerställa jämn kvalitet hos nålarna.

Abstract [en]

Testing the particle emission from studded tire wear of road surfaces in a controlled manner is usually associated with realistic, but large-scale tests with large-scale and advanced laboratory equipment and thus relatively high costs. There is therefore an urgent need for a simpler method that can be used to provide a reasonable and good estimate of how differences in coating recipes affect particle formation, which can be used to select coating recipes to be used in later large-scale tests. One possibility is to use an existing wear test method for wear bearing specimens. Tröger is such a method where a bundle of steel needles hammers against a rotating sample body in a climate cabinet deemed suitable for measuring and studying particle emissions into air. VTI's Tröger equipment was modified for particulate emission measurements by installing particulate suction nozzles in the cooling airflow passing over the specimen. Initial tests indicated acceptable/sufficiently good repeatability and a number of specimens from some existing materials with different wear resistances were selected for further testing. A statistically optimized trial plan and sample handling was developed. One test round was planned initially but later it was expanded to two rounds. A second round was required partly because a material in the first round was mistaken for being too uniform, but consisted of three different materials, partly because the trial set-up could be improved somewhat. The particles formed (PM10) have a bimodal distribution with a primary peak at 2–3 µm and a secondary one at about 8–10 µm. The statistical analysis showed significant differences between the three constituent materials in the test bodies in the second test round and that the method in its current form can be used to distinguish the particle emission from different road surfaces. Suggestions for developing the method include preventing the build-up of dust in the cooling system and ensuring consistent quality of the needles.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2023. p. 46
Series
Trafikverkets forskningsportföljer
Keywords
PM10, slitage, vägbeläggning, Tröger, metodutveckling, dubbdäck
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Vidmakthålla
Identifiers
urn:nbn:se:trafikverket:diva-16306 (URN)
Projects
BVFF Indikativ metod för bedömning av vägbeläggningars generering av slitagepartiklar
Funder
Swedish Transport Administration, TRV 2018/99035
Available from: 2024-08-29 Created: 2024-08-29 Last updated: 2025-09-04
Lundberg, T., Carlson, A., Eriksson, O., Genell, A., Ihs, A., Janhäll, S., . . . Wennström, J. (2022). Indikatorer för Trafikverkets uppföljning av underhåll på belagda vägar: leveranskvaliteter för de transportpolitiska målen. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Indikatorer för Trafikverkets uppföljning av underhåll på belagda vägar: leveranskvaliteter för de transportpolitiska målen
Show others...
2022 (Swedish)Report (Other academic)
Alternative title[en]
Indicators for the Swedish Transport Administration's follow-up of maintenance on paved roads : delivery qualities for the transport policy goals
Abstract [sv]

Ett sätt för Trafikverket att följa upp effekterna av underhållet på de statliga vägarna är genom att använda sig av indikatorer. De indikatorer som beskrivs i denna rapport benämns som andra ordningens indikatorer och byggs upp av underliggande data. Indikatorerna som vi valt att arbeta med ska på ett allsidigt och transparent sätt beskriva hur Trafikverket uppfyller leveranskvaliteten för punktlighet, kapacitet, robusthet, användarbarhet, säkerhet samt miljö och hälsa.

 I denna förstudie sammanfattar vi en kunskapsöversikt för valda indikatorer och förslag på hur de kan implementeras i Trafikverkets pavement management system. De indikatorer som vi arbetar med är Säkerhet, Komfort, Strukturellt tillstånd, Rullmotstånd, Buller, Luftkvalitet, Godsskador, Ytskador, Fordonsslitage och slutligen en indikator för Hälsa. Det finns många aspekter att ta hänsyn till då en indikator introduceras. Den absolut viktigaste är, bortsett från att den är validerad, att den får acceptans och används. Det finns många sätt att använda en indikator och att enbart titta på absoluta värden är svårt för en sammansatt indikator. Relativa skillnader vid årliga uppföljningar är att föredra för att avgöra om strategier får avsedd effekt.

Abstract [en]

One way for the Swedish Transport Administration (STA) to follow up the effects of maintenance on state roads is by using indicators. The indicators described in this report are defined as second-order indicators and are built up using underlying data. The indicators describe, in a comprehensive and transparent way, how the STA meets delivery quality parameters for punctuality, capacity, robustness, usability, safety, and environment and health. 

In this feasibility study, a knowledge overview of the selected indicators is presented. Suggestions are also given on how the indicators can be implemented in the STA's pavement management system. The indicators studied were Safety, Comfort, Structural Condition, Rolling Resistance, Noise, Air Quality, Goods Damage, Surface Damage, Vehicle Wear, and Health Risk. Many aspects must be considered when introducing an indicator. Along with validation, it is extremely important that the indicator will be accepted and used. There are many ways to use an indicator, however, it is not ideal to only consider absolute values for a composite indicator. Relative differences in annual follow-ups are preferable to determine whether strategies have the intended effect.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2022. p. 91
Series
Trafikverkets forskningsportföljerTrafikverkets forskningsportföljerTrafikverkets forskningsportföljer
Keywords
Pavement management, indikator, vägunderhåll, vägytans tillstånd
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Vidmakthålla
Identifiers
urn:nbn:se:trafikverket:diva-16282 (URN)
Projects
Indikatorer i Trafikverkets Pavement Management System
Funder
Swedish Transport Administration, TRV 2015/75559
Available from: 2024-08-23 Created: 2024-08-23 Last updated: 2025-09-04
Eriksson, J., Eriksson, O., Silvano, A. P. & Karlström, J. (2022). Skattning av cykeltrafikarbetet: en pilotstudie i tre kommuner. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Skattning av cykeltrafikarbetet: en pilotstudie i tre kommuner
2022 (Swedish)Report (Other academic)
Alternative title[en]
Estimation of the kilometers travelled by bicycle : a pilot study in three different municipalities in Sweden.
Abstract [sv]

Nationellt (via gång- cykel- och kollektivtrafikmålet), regionalt och i många av Sveriges kommuner finns målsättningar om ökad cykling. Dessa målsättningar är dock svåra att följa upp, då cykeltrafikens storlek inte mäts och följs upp. Med de metoder som används idag för flödesmätningar är det inte möjligt att skatta cykeltrafikarbetet i hela kommunen, då flödesmätningarna inte genomförs på systemnivå för det cykelbara vägnätet. Det övergripande syftet med pilotstudien är att ta fram en accepterad, tillförlitlig, tillämpbar och enhetlig metod för att skatta cykeltrafikarbetet i kommunen genom flödesmätningar. 

Kommunerna Stockholm, Uppsala och Östersund ingår i pilotstudien. Det genomfördes 135 veckomätningar i varje kommun; 100 på gång- och cykelvägnätet och 35 i blandtrafik, uppdelat på fem etapper. De kontinuerligt mätta flödespunkterna användes som information för uppräkning på helårsnivå. Cykelvägnätet omfattar inte grusvägar, enskilda väghållare och vägar med skyltad hastighet 80 km/h och högre. Länkarna delades in i stratum, där det i varje stratum gjordes ett systematiskt urval på den totala länklängden. Skattningsmetoden tog hänsyn till både rum och tid. 

Under det brutna året vecka 35 år 2020 till vecka 34 år 2021 cyklades det 145±43 miljoner kilometer i Stockholm, 59±23 miljoner kilometer i Uppsala och 9±3 miljoner kilometer i Östersund. Osäkerheten i skattningen, utgör mellan 30 och 40 procent av punktskattningen. Det är en ganska stor osäkerhet i skattningen, men tillräckligt liten för att se att det exempelvis är skillnader mellan kommunerna. 

Något som framkommit i denna studie är att cyklandet i blandtrafik inte är försumbar och kommunerna bör ha detta i beaktande. För att studien ska komma till sin rätt bör den upprepas en gång till i minst en av dessa kommuner.

Abstract [en]

Nationally (by the walking, cycling and public transport target), regionally and in many of Sweden's municipalities there are targets for increased cycling. However, these objectives are difficult to follow up, as the amount of bicycle traffic is not measured and followed up. The overall aim of the pilot study is to develop an accepted, reliable, applicable, and uniform method for estimating the kilometers travelled by bicycle in the municipality through bicycle flow measurements. 

The municipalities of Stockholm, Uppsala and Östersund are included in this pilot study. 135 weekly measurements were carried out in each municipality; 100 on the pedestrian and bicycle road network, 35 in mixed traffic, divided into five periods. The year-round measured cycle flow measurements were used as information for enumeration at year-round level. The cycle path network does not include gravel roads, individual road holders and roads with a speed limit of 80 km/h and higher. The links were divided into strata, where a systematic selection of the total link length was made in each stratum. The estimation method considered both space and time. 

During the year week 35 of 2020 to week 34 of 2021, 145±43 million kilometers were cycled in Stockholm, 59±23 million kilometers in Uppsala and 9±3 million kilometers in Östersund. The uncertainty in the estimate constitutes between 30 and 40 percent of the point estimate. There is a fairly large uncertainty in the estimate, but small enough to see that there are, for example, differences between the municipalities. 

Something that emerged in this study is that cycling in mixed traffic is not negligible and the municipalities should take this into account. The study should be repeated once more in at least one of these municipalities.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2022. p. 54
Series
Trafikverkets forskningsportföljer
Keywords
Cykeltrafikarbete, cykelflöde, cykelflödesmätningar, cykelmätningar
National Category
Transport Systems and Logistics
Research subject
FOI-portföljer, Planera
Identifiers
urn:nbn:se:trafikverket:diva-16284 (URN)
Projects
SKR Enhetlig metod för cykelflödesmätningar – en pilotstudie
Funder
Swedish Transport Administration, TRV 2019/138572
Available from: 2024-08-23 Created: 2024-08-23 Last updated: 2025-09-04
Mirzadeh, I., Eriksson, O. & Lundström, R. (2020). Performance requirements in design-build contracts: development of a risk assessment model. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Performance requirements in design-build contracts: development of a risk assessment model
2020 (English)Report (Other academic)
Alternative title[sv]
Funktionella krav i totalentreprenader : utveckling av en modell för riskbedömning
Abstract [en]

The gradual shift in procurement of road infrastructures from traditional design-bid-build (DBB) to design-build (DB) contracts, have resulted in an ever-increasing need for contractors and consultants to assess and predict the technical performance of selected designs and corresponding risks. Moreover, there is a great interest for the road administration to better motivate the type of contract and the procurement strategy based on risks and outcomes in road projects. This report has focused on developing a model for evaluation of the impact of performance requirements in DB and design-bidmaintain (DBM) projects. The model can analyse the risk of exceeding the maximum requirements during the warranty period. Therefore, it can be applied by contractors for evaluation of the technical risk not only at the bidding stage but also during the warranty period. It can also be used by the road administration as a decision support tool for setting performance requirements at the project level.

Abstract [sv]

Gradvis utveckling eller förändringar inom upphandlingspraxis, exempelvis från traditionella utförandeentreprenader till totalentreprenader, har resulterat i ständigt större behov för entreprenörer och konsulter att kunna bedöma och prediktera teknisk prestanda hos valda konstruktioner, material och utförandemetoder. På ett motsvarande sätt finns det ett stort intresse hos beställare av infrastrukturprojekt att kunna bättre motivera val av entreprenadform och upphandlingsstrategi baserat på risker och tidigare utfall i entreprenadprojekt. Denna rapport har fokuserat på utveckling av en modell för analys av funktionskravens påverkan i totalentreprenader från Trafikverket och entreprenörernas perspektiv. Modellen kan analysera risken för att funktionskraven ska överskridas under garantitiden. Den kan därför användas av entreprenörer för utvärdering av den tekniska risken vid anbudsskedet och även under garantitiden. Modellen kan även användas av Trafikverket som ett beslutsstödsverktyg vid kravställning.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2020. p. 39
Series
Trafikverkets forskningsportföljer
National Category
Economics and Business Infrastructure Engineering
Research subject
FOI-portföljer, Bygga
Identifiers
urn:nbn:se:trafikverket:diva-5658 (URN)
Projects
BVFF Ökad produktivitet i vägsektorn genom effektivare riskbedömning i samband med totalentreprenader
Funder
Swedish Transport Administration, TRV 2017/62623
Available from: 2022-10-27 Created: 2022-10-27 Last updated: 2025-09-04
Arvidsson, A. K., Lundberg, T., Kalman, B., Ekström, C., Cruz del Aguila, F. & Eriksson, O. (2019). Friktions- och texturutveckling på nya beläggningar. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Friktions- och texturutveckling på nya beläggningar
Show others...
2019 (Swedish)Report (Other academic)
Alternative title[en]
Friction and texture developments on new paving
Abstract [sv]

En ny vägyta bör vara och upplevas som säker av trafikanterna oavsett vilket väglag som råder. Det är därför viktigt att vägbanan har en tillfredställande nivå på friktion redan när vägen öppnas. Det finns begränsade dokumenterade kunskaper hur vägen förändras den första tiden efter en beläggningsåtgärd.

Syftet med detta projekt är att fastställa hur friktionen förändras under den första tiden efter att vägbeläggningen är lagd och trafikpåsläpp sker. Ambitionen är att kunna avgöra om nylagda vägavsnitt har nedsatt friktion och ge rekommendationer för när en friktionsmätning ska utföras och hur skyltning ska ske i anslutning till beläggningsarbeten. Upplägget har varit att följa olika objekt med täta friktions- och texturmätningar från strax innan trafikpåsläpp tills nivåerna har stabiliserats.

Initialt är friktionen hög för att sen avta med mängden trafik. Efter 1–3 veckor nåddes det lägsta värdet och därefter ökade eller stabiliserades friktionen. Gemensamt för alla undersökta sträckor var att det sker stora förändringar i texturnivåerna från att det första fordonet trafikerar vägen och därefter är den starkaste tendensen en sjunkande texturnivå tills en stabil nivå uppnås efter 1–3 veckor.

Abstract [en]

A new pavement should be and be perceived as safe by road users, regardless of the road condition. It is therefore important that the road has a satisfactory level of friction already when the road is opened. There is limited documented knowledge of how the road change in the beginning after a paving performance.

The purpose of this project is to determine how friction changes during the first period after road pavement is laid and traffic is permitted. The ambition is to determine if new road sections have reduced friction and provide recommendations for when a friction measurement is to be performed, and how warning signs should be displayed in connection with the pavement work. The study plan has been to follow different objects with frequent friction and texture measurements from just before the stretch is opened for traffic until the levels have stabilised.

Initially, friction is high, and then decreases with the amount of traffic. After 1-3 weeks the lowest value was reached and then the friction increased or stabilized. Common to all investigated stretches, there are major changes in texture levels from the first vehicle and then a decreasing textural level until a stable level is reached after 1-3 weeks.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2019. p. 80
Series
Skyltfonden
Keywords
Friction, Surface texture, Surfacing, Time, Change, Skidding resistance, Measurement, Field (test), Laboratory (not an organization), Test, Bituminous mixture, Friktion, textur, beläggning, olyckor
National Category
Infrastructure Engineering
Research subject
Skyltfonden, Skyltfonden - Vägen och trafikmiljön
Identifiers
urn:nbn:se:trafikverket:diva-5567 (URN)
Funder
Swedish Transport Administration, TRV 2015/85046
Note

Rapporten är framtagen med ekonomiska bidrag från Trafikverket, Skyltfonden. Ståndpunkter och slutsatser i rapporten reflekterar författaren och överensstämmer inte med nödvändighet med Trafikverkets ståndpunkter och slutsatser inom rapportens ämnesområden.

Available from: 2022-10-05 Created: 2022-10-05 Last updated: 2025-09-04
Arvidsson, H. & Eriksson, O. (2019). Jämförande provning – grovsiktning: ballast 2018. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Jämförande provning – grovsiktning: ballast 2018
2019 (Swedish)Report (Other academic)
Alternative title[en]
Interlaboratory comparison – coarse material sieving : aggregate 2018
Abstract [sv]

Detta notat redovisar resultat, precisionsdata och viss statistisk analys från jämförande provning mellan ett antal laboratorier i Sverige.

Analys angående påverkan av ackreditering eller inte, har inte gjorts då det inte efterfrågats i svarsunderlaget. Troligen är de flesta deltagarna ackrediterade med få undantag, så eventuell statistisk analys hade haltat.

För grovsiktningen, siktning av material på sikt 16 mm och grövre, är spridningar (standardavvikelser ca 0,7 %-enheter) och differenser mellan maximala och minimivärden (ca 3–4 %-enheter) små.

För resultat av material finare än 16 mm (i förhållande till hela kurvan) så är spridningarna större (stora). Framför allt för siktarna i spannet 1–11,2 mm. Där är skillnaden mellan max- och min-värden uppåt 7 %-enheter och standardavvikelsen uppåt 1,4 %-enheter. För siktar finare än 1 mm är spridningar (standardavvikelser ≤ 0,8 %-enheter) och differenser (≤ 3 %-enheter) mer acceptabla.

Spridningar är större för finsiktning än för grovsiktningsdelen vilket kan misstänkas bero på större variation i provmaterialet som kommer från asfaltssorteringar (sorteringarna 0/4, 4/8, 8/11 och 11/16 mm). Det har även tillkommit ett (eller flera) moment som neddelning av material 0–16 mm vilket också kan bidra till större spridning.

Abstract [en]

This report shows results, some statistical analysis and precision data for interlaboratory comparison (round robin) in Sweden performed on a proportioned base layer material of crushed rock for grain size distribution according to TDOK 2014:0145 (coarse material sieving) and EN 933-1:2012 (sieving on 0/16 mm).

There were 48 laboratories participating.

In the sieving on coarse material, ≥ 16 mm, the deviations are small (standard deviations approx. 0,7%) and the difference between maximum and minimum value for each sieve is only 3–4%.

The results for material finer than 16 mm (relatively to whole of the sample) are deviations wider. Especially for sieves 1/11,2 mm with difference between maximum and minimum values are up to 7% and the standard deviation for those sieves are around 1,4%. For sieves finer than 1 mm (0,5 mm and less) the differences are less than 3% and the standard deviation is less than 0,8%.

The spreading’s for the fine material sieving is wider than for the coarse sieving part. It could depend on less accurate gradings on the fractions finer than 16 mm that were used in the proportioning. For the coarse sieving the whole sample (18 kg) were the test portion, for the fine sieving the material 0/16 mm had to be divided to get the test portion (approx. 2,6 kg). The dividing can also be one of the reasons to less accurate results for the 0/16 mm-part.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2019. p. 43
Series
Trafikverkets forskningsportföljer
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Bygga
Identifiers
urn:nbn:se:trafikverket:diva-5634 (URN)
Projects
BVFF - Jämförande provning av vägmaterial
Funder
Swedish Transport Administration, TRV 2017/119795
Available from: 2022-10-17 Created: 2022-10-17 Last updated: 2025-09-04
Lundberg, T., Eriksson, O. & Glantz, C. (2019). Kontroll och uppföljning av entreprenader - del 2, tillståndsutveckling, mätfel och risker: Vägytemätning med mätbil. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Kontroll och uppföljning av entreprenader - del 2, tillståndsutveckling, mätfel och risker: Vägytemätning med mätbil
2019 (Swedish)Report (Other academic)
Alternative title[en]
Control and follow-up of contracts - part 2, condition development,measurement errors and risks : Road surface measurement
Abstract [sv]

Trafikverket har som mål att öka antalet totalentreprenader. För att få en fungerande kontrollapparat kring entreprenaderna krävs metoder för att verifiera att ställda krav uppfylls under vägens garantitid. I denna undersökning riktar vi in oss på funktionella krav som ställs vid totalentreprenader och som kan kontrolleras med vägytemätning.

Rapporten belyser mätfel vid objektmätning (kontrollmätning). Mätfelet delas upp i olika komponenter: slumpmässiga, systematiska och variation mellan olika leverantörer. Även riskbedömning berörs där beräkningar av risken för felbedömning av en sträcka presenteras.

Slutligen presenteras hur jämnheten vid anläggningen av en entreprenad påverkar vägens framtida tillståndsutveckling och vilka initialvärden vi kan förvänta oss på en totalentreprenad och underhållsbeläggning. Vi ser att en väg med god jämnhet längs och tvärs färdriktningen ger lägre utvecklingstakt under beläggningens livslängd.

Abstract [en]

The Swedish Transport Administration aims to increase the number of design build contracts. To get a functioning control device around the contracts, well defined requirements must be set for the warranty period of the road. In this survey we focus on functional requirements that are set for design build contracts and which can be checked by means of a road surface testing.

In the report, measurement errors are highlighted in object measurement (control measurement). The measurement error is divided into different components: random, systematic and variation between different suppliers. Risk assessment is also discussed where calculations of the risk of error assessment of a section are presented.

Finally, it is presented how the results of the condition (evenness) affect the future development of the road and what initial values we can expect from a design build contract and maintenance work. We see that a road of good evenness, longitudinally and transversally, gives a lower development rate during the life of the road.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2019
Series
Trafikverkets forskningsportföljer
Keywords
Surfacing, Condition survey, Evenness, Rut, Measurement, Method, Accuracy, Error, Quality assurance, Road construction, Contract
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Vidmakthålla
Identifiers
urn:nbn:se:trafikverket:diva-5741 (URN)
Projects
Objektiv kontroll vid funktionsåtaganden, tillståndsvärdering av vägytan
Funder
Swedish Transport Administration, TRV 2012/58359
Available from: 2023-02-06 Created: 2023-02-06 Last updated: 2025-09-04Bibliographically approved
Eriksson, O. & Andrén, P. (2019). Prognosmetoder för spårdjup och IRI: vägytedata 1997–2016. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Prognosmetoder för spårdjup och IRI: vägytedata 1997–2016
2019 (Swedish)Report (Other academic)
Alternative title[en]
Prediction methods for rut depth and IRI : road surface data 1997–2016
Abstract [sv]

Rapporten presenterar ett förslag till en prognosmetod för framtida värden av spårdjup och IRI på det belagda statliga vägnätet samt olika mått på prognosnoggrannhet. Metoden kan även användas för att fylla i saknade värden bakåt i tiden.

En tidigare VTI rapport inom samma område kom fram till att ett prognosunderlag endast ska innehålla information om utvecklingen lokalt och baserade sin prognos på data endast från den senaste beläggningsomgången. En väsentlig förändring här är att metoden utvidgats till att inkludera data från tidigare beläggningsomgångar i prognosberäkningen, med redovisning av de för- och nackdelar som det medför. Andra delar, t.ex. hur data förbereds, har inte ändrats i någon större utsträckning.

Resultaten blir i huvudsak att prognoser inte blir tydligt bättre generellt, inte heller tydligt sämre, av att ta med data från tidigare beläggningsomgångar. Det finns ändå en fördel med att ta med dem därför att fler sträckor över huvud taget kan få en prognos baserad på lokala förutsättningar.

Abstract [en]

This report presents a proposal for a prediction method for future values of rut depth and IRI on the paved state road network and various measures of forecast exactness. The method can also be used to fill in missing values backward in time.

An earlier VTI report within the same area concluded that a prediction method should use only data about the development locally and based its prediction on data from the current pavement cycle only. A major difference here is that the method has been expanded to include data from previous pavement cycles in the prediction method, with presentation of the advantages and disadvantages that this entails. Other parts, e.g. how data is prepared, has not been changed in any great extent.

The results are mainly that forecasts do not generally become clearly better, nor clearly worse, by including data from previous pavement cycles. There is nevertheless an advantage in including these data because that makes prediction based on local conditions possible for more sections.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2019. p. 99
Series
Trafikverkets forskningsportföljer
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Äldre portföljer
Identifiers
urn:nbn:se:trafikverket:diva-5587 (URN)
Projects
Prognosmodeller för tillståndsmått 2013-2015
Funder
Swedish Transport Administration, TRV 2012/52572
Available from: 2022-10-05 Created: 2022-10-05 Last updated: 2025-09-04
Arvidsson, H. & Eriksson, O. (2018). Jämförande provning – ballast 2017: micro-Deval och Los Angeles. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Jämförande provning – ballast 2017: micro-Deval och Los Angeles
2018 (Swedish)Report (Other academic)
Alternative title[en]
Interlaboratory comparison - aggregate 2017
Abstract [sv]

Detta notat redovisar resultat, precisionsdata och viss statistisk analys från jämförande provning mellan ett antal laboratorier i Sverige. De metoder som ingått i analysen har varit: motstånd mot nötning, micro-Deval (våt) enligt SS-EN 1097-1 och motstånd mot fragmentering, Los Angeles enligt SS-EN 1097-2. Antalet deltagande laboratorier har varit 37 för micro-Deval respektive 34 för Los Angeles.

Tre material ingick den jämförande provningen (ringanalysen). De levererades i sorteringarna 8/11 mm och 11/16 mm. Laboratorierna skulle ur dessa sorteringar framställa analysfraktionen 10–14 mm.

Resultaten för micro-Deval var snarlik för alla tre materialen med medelvärden i intervallet 6–8. Likaså var det snarlika nivåer för spridningen (standardavvikelsen) för de tre materialen.

För Los Angeles hade ett material medelvärdet 12 de andra två hade medelvärden kring 26–27. Nivåer för spridningarna följer medelvärden vilket även visar sig i variationskoefficienten som ligger på ca 5-6 %.

Abstract [en]

This report shows results, some statistical analysis and precision data for interlaboratory comparison (round robin) in Sweden performed on three materials of aggregate during 2017. The properties that was determined was resistance to wear by wet micro-Deval test (EN 1097-1) and resistance to fragmentation, Los Angeles test (EN1097-2). The number of participating laboratories were for micro- Deval 37 pcs. and for Los Angeles 34 pcs.

There were three materials used for this comparison, the materials were called F, S and V. They were delivered to the participating laboratories in the grading 8/11 mm and 11/16 mm for each material. The laboratories should then generate the proper analyze fraction of 10/14 mm.

The average results for micro-Deval were at the range of 6–8 for all of the materials. The standard deviations were also similar (0,43–0,50).

For Los Angeles there were the average for one of the materials at 12 and for the other two materials the averages were around 26–27. The standard deviations are proportional to the averages.

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2018. p. 44
Series
Trafikverkets forskningsportföljer
Series
VTI notat ; 18-2018
Keywords
Test method, Group analysis (test), Aggregate, Properties, Los Angeles test, Wear, Laboratory (not an organization)
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Bygga
Identifiers
urn:nbn:se:trafikverket:diva-5628 (URN)
Funder
Swedish Transport Administration, TRV 2015/34720
Available from: 2022-10-14 Created: 2022-10-14 Last updated: 2025-09-04
Lundberg, T., Andrén, P., Wahlman, T., Eriksson, O., Sjögren, L. & Ekdahl, P. (2018). Ny teknik för vägytemätning: tvärprofil och spårdjup. Linköping: Statens väg- och transportforskningsinstitut
Open this publication in new window or tab >>Ny teknik för vägytemätning: tvärprofil och spårdjup
Show others...
2018 (Swedish)Report (Other academic)
Alternative title[en]
New technology for road surface measurement : transverse profile and rut depth
Abstract [sv]

I Sverige och Finland mäts tillståndet på det statliga belagda vägnätet årligen. Mättekniken har varit densamma under en lång tid vilket har sina fördelar. I och med att mätningarna utförs med samma mätteknik bibehålls trender och mätserier utan störningar. Den nuvarande tekniken är dessutom driftsäker och kan handlas upp till en prisnivå som genom åren snarare sjunkit än ökat. Det huvudsakliga användningsområdet för tillståndsmätningen är att förse underhållsverksamheten med ett objektivt underlag för beläggningsplaneringen, men när det visar sig att nuvarande objektiva tillståndsdata endast kan förklara mellan 40 och 75 procent (beroende av trafikklass) av de åtgärder som verkligen görs på vägnätet, måste det övervägas om denna ska kompletteras med nya tillståndsdata. Den information som saknas tros vara information om ytskador och sprickor. Detta kräver ny mätteknik.

Om ny teknik ska börja anammas, för insamling av tillståndsdata, måste först de grundläggande mätstorheternas tillförlitlighet säkerställas, innan nya möjligheter och mätstorheter undersöks. Denna studie är därför endast inriktad på tvärprofilmätning och mått för ojämnhet i tvärled (spårdjup och spårrygg).

I studien har två av de ledande nya teknikerna som arbetar med skannande laser undersökts, LCMS från Pavemetrics och PPS från Fraunhofer. Resultatet av studien visar att tekniken är bra, noggrannhet och repeterbarhet går att jämföra med de nuvarande punktlasersystemen. Kriterier och krav för upphandling av mättjänster där den nya tekniken används bedöms också kunna bibehållas.

Abstract [en]

The condition of the national coated road network is measured annually in Sweden and Finland. The measuring technology has been unchanged over a long period of time, which has its benefits. As the measurements are performed using the same technology, trends and measurement series are retained without any disruption. In addition, the technology currently used is reliable and can be procured at a price level that has fallen rather than risen over the years. The principal area of use for condition measurement is to provide maintenance work with an objective basis for the planning of surfacing, but when it is found that current objective condition data can only explain between 40 and 75 percent (depending on class of traffic) of the action actually taken on the road network, consideration must be given to whether new condition data need to be added. The information that is lacking is thought to be information on surface damage and cracks. This requires new measuring technology.

If new technology will be adopted, for the collection of condition data, the dependability of the basic measured quantities must be ensured before new options and measured quantities are examined. This study is therefore focused only on transverse-profile measurement and measures of unevenness in the transverse direction (rut depth and ridge height).

The study has examined two of the leading new technologies that operate with scanning lasers, LCMS from Pavemetrics and PPF from Fraunhofer. The outcome of the study shows that the technology is good, and that accuracy and repeatability are comparable to the present-day point-laser systems. It is also deemed possible to retain criteria and requirements for the procurement of measurement services when the new technology is used

Place, publisher, year, edition, pages
Linköping: Statens väg- och transportforskningsinstitut, 2018. p. 136
Series
Trafikverkets forskningsportföljer
Keywords
Surfacing, Rut, Transverse profile, Measurement, Method, Apparatus (measuring), Laser, Sensor, Condition survey, Specifications, Finland, Sweden
National Category
Infrastructure Engineering
Research subject
FOI-portföljer, Bygga
Identifiers
urn:nbn:se:trafikverket:diva-5503 (URN)
Projects
Beskrivning av metod och utvecklingsmöjligheter för vägytemätning
Funder
Swedish Transport Administration, TRV 2016/56661
Available from: 2022-09-28 Created: 2022-09-28 Last updated: 2025-09-04
Organisations
Identifiers
ORCID iD: ORCID iD iconorcid.org/0000-0002-5306-2753

Search in DiVA

Show all publications